Progressive Generators For Thin Film Solar Cell Applications

This article looks into some of the aspects regarding thin film solar applications, with special emphasis on generators for sputter deposition, modular DC systems, arc management and generators for PECVD coating. High precision process control and supreme arc management, with adaptable parameters to provide minimal disturbances in the plasma process and to obtain optimised results in terms of film quality, homogeneity and uniformity over the whole substrate must be respected.

Author
D Ochs & T Rettich
Origin
Huttinger Gmbh, Germany
Journal Title
Glass Coatings 2/2006 25-29
Sector
Flat glass
Class
F 2073

Request article (free for British Glass members)

Progressive Generators For Thin Film Solar Cell Applications
Glass Coatings 2/2006 25-29
F 2073
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.