Production Of Metallic Glazes And Their Industrial Applications

Metallic glazed and decorated tiles are the latest trend in which special printing bases, granules and glazes are used. The aim of this study was to develop metallic glazes for wall tiles by developing new, alternative glass-ceramic glaze system.