Production Of Flint Glass From Raw Materials

Quartz from the Visheritsa deposit in Bulgaria and Zn oxide and precipitated CaCO3 manufactured in that country may be used successfully for the production of high-quality flint glass, but the native Pb oxide, potash, BaCO3, dolomite, and other raw materials are unsuitable.

Author
E. Vodenicharova Et Al.
Origin
Unknown
Journal Title
Stroit. Materiali Silikat. Prom,. [4] 31-34 (1964)
Sector
Primary Papers
Class
PP 367

Request article (free for British Glass members)

Production Of Flint Glass From Raw Materials
Stroit. Materiali Silikat. Prom,. [4] 31-34 (1964)