[Processing] Synthetic Coolants Enhance Glass Grinding Process

When processing glass with diamond tools, the use of a synthetic (mineral oil-free) coolant offers several advantages. In this article the author, Dr Michael Emonds from German-based Aachener Chemische Werke, gives a closer look at he grinding process, describing the different features of coolants and how they can improve the efficiency of the drilling process.