[Processing] Free Forms And Models Cut From Laminated Glass

With its ProLam Plus innovation, German-based HEGLA has unveiled a cutting system with which free forms and models can be cut automatically and with precision from laminated safety glass.

Author
C Koch
Origin
Hegla
Journal Title
Glass Worldwide Sept-Oct 2013 56-57
Sector
Flat glass
Class
F 3448