Primary Techniques To Reduce Nox Emissions From A Float Furnace

Saint-Gobain, in partnership with ADEME, has conducted research into methods of controlling nitrogen oxide emissions from the float glass furnace through a series of primary measures. The Saint-Gobain plant in Aniche was the starting point for the research and recent results are presented in this article.