Premadia For Edge Grinding Glass

The application of the PremaDia concept, by which grit particles are assigned an indicator value to describe key characteristics, is discussed in this paper with reference to the selection of diamond abrasive for the edge grinding of glass.

Author
Dipl. Ing. H O Juchem
Origin
Unknown
Journal Title
Industrial Diamond Review 3/95 112-115
Sector
Flat glass
Class
F 528