Preheating Of Raw Materials And Combustion Air With Cfb (Circulating Fluidized Bed) Heat Exchanger

A new glass furnace energy recovery system based on Regenerative Circulating Fluidized Bed technology is proposed and discussed in this paper. Operating and control principles of RCFB units as well as results from preliminary test runs will be introduced.

Author
J Ristola & S Ruotti
Origin
Rihimaen Lasi Oy & Einco Oy, Finland
Journal Title
Glasteknisk Tidskrift 49 2 1994 60-62
Sector
General
Class
G 1249

Request article (free for British Glass members)

Preheating Of Raw Materials And Combustion Air With Cfb (Circulating Fluidized Bed) Heat Exchanger
Glasteknisk Tidskrift 49 2 1994 60-62
G 1249