Prediction Of Elastic Strains In Adhesively Bonded Diamond Optical Disks

An elastic strain numerical model was used to predict the stresses, radius of curvature and deflection of thick diamond films bonded at elevated temperatures to silicon, germanium and zinc sulphide substrates.