Pre-Coats And Delivery Coatings

This article gives a background to the problems presented by traditional pre-coats and delivery coatings and then describes the development, application and advantages of Kleenmould Precoat 100, a dual-purpose, water-based, non-hazardous blank/mould pre-coat and delivery equipment coating.