Possibilities Of Using The Nondestructive Activation Analysis With 14 Mev Neutrons In The Investigation Of Glass

This paper describes the principle of neutron analysis as well as the apparatus in detail. The authors emphasise that in its application for the analysis of glass, the apparatus must be adapted for the simultaneous analysis of several atomic species. Also in order to increase its efficiency it should be coupled to ad programmer for quick results.