Possibilities Of Automated Glass Flaw Monitoring On Running Float Glass Ribbon And Flat Windshield Templets

The physics of automatic methods of on-line inspection of a float glass line are discussed. A laser scanner based on computer-aided signal evaluation, defect-size classification and link to an on-line cut-optimising computer is described.