Port Geometry And Flame Shape In Glass Melting Furnaces

Model experiments on optimum burner systems and port design are described.

Author
A Grossman
Origin
State Glass Research Institute, Hradec Kralove
Journal Title
Glastech Ber 1989 62 7 231-233
Sector
General
Class
G 282