Picking Up Tin Defects In Flat Glass

As tin is a problem for coating and further processing of flat glass, Innomess has developed a tin detection channel that enhances the powerful Floatscan-Catcher & Optics defect detection system. The tin channel detects and characterises even the smallest tin defects on the top or bottom of the float ribbon, allowing the detection of any type of tin defects at the earliest possible stage on the float line.