Photocoloumetric Method For Determining Microquantities Of Fluorine In Quartz Glass

A method has been developed for determining very small amounts of fluorine in phosphate-silica with sufficient accuracy for contents of 0.01-0.08%. The technique requires 6 hours to complete.

Author
A.M. Kaplunova Et Al.
Origin
Unknown
Journal Title
Glass And Ceramics 1980 37 (3-4) 209-210