Phase Relations In The Cu0-Pb0-B203 System

Phase equilibria in the Cu0-Pb0-B203 system are studied by standard physico-chemical characterization techniques (thermal analysis, x-ray diffraction, density, microhardness, resistivity, thermal expansion, and dielectric permittivity measurements).

Author
M I Zargarova Et Al
Origin
Unknown
Journal Title
Inorg Mater 33 10 1997 1046-1051