Packaging Technology In Glasswork Industry - General Questions On The Handling And The Packaging Of Glass Containers In The Cold End

This paper analyses many questions regarding the handling and packing of glass containers.

Author
M Fallini
Origin
Unknown
Journal Title
International Glass Journal No.. 82 1994 40-50