Oxy-fuel applications in the glass industry are enabling performance increases, fuel savings, environmental benefits and improvements in overall melter operation. Air Products combines a wide range of delivered and on-site oxygen supply schemes with its dedicated in-house glass industry technical team supported by centre-of-excellence combustion laboratories, a thorough knowledge of industrial combustion processes, a fluid dynamics model capability and specific knowledge of the glass maker's melting requirements.

Author
A Ratti
Origin
Air Products
Journal Title
Glass Worldwide July-August 2015 84-86
Sector
General
Class
G 4371

Request article (free for British Glass members)

Oxy-Fuel Technology And The Glass Container Industry
Glass Worldwide July-August 2015 84-86
G 4371
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.