Oxy-Fuel Tableware Furnace With Novel Oxygen- And Natural Gas Preheating System

As the global demand for natural gas continues to rise and environmental regulation targets are becoming increasingly stringent, glass manufacturers are faced with the challenge of reducing costs for melting glass under a variety of operating constraints without compromising glass quality and productivity. This enabled a stronger demand among glass manufacturers to invest in innovative waste heat recovery schemes and energy-and emission reduction technologies. This article describes how Air Liquide's Alglass HeatOx technology was implemented at its 200/tpd tableware furnace in Bulgaria.

Author
T Goruney Et Al
Origin
Sisecam R&D, Turkey
Journal Title
77 Conf On Glass Problems 38 1 2017 73-83
Sector
Domestic glass
Class
D 1428

Request article (free for British Glass members)

Oxy-Fuel Tableware Furnace With Novel Oxygen- And Natural Gas Preheating System
77 Conf On Glass Problems 38 1 2017 73-83
D 1428
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.