Oxy-Fuel Melter Combined With Waste Heat Recovery System

Heye-Glas has pioneered the use of waste heat recovery equipment with its conventionally fired glass melting furnaces in recent years. Now the company has developed the concept further to work with oxy-fuel melting installations.

Author
D Portner & H G Frieg
Origin
Heye-Glas , Germany
Journal Title
Glass 73 6 1996 233
Sector
Container glass
Class
C 956