Oxy-Fuel Furnace Design Considerations

Standardisation of oxy-fuel furnace design principles is a difficult task as there are a wide variety of glass furnace configurations and operating conditions. To ensure the success of such a furnace, specific evaluations must be performed.

Author
R Ruiz Et Al
Origin
Air Liquide America Corp, Usa
Journal Title
Glass Industry 76 6 May 1995 10, 13-14, 19-20, 23
Sector
General
Class
G 1269

Request article (free for British Glass members)

Oxy-Fuel Furnace Design Considerations
Glass Industry 76 6 May 1995 10, 13-14, 19-20, 23
G 1269