Oxy-Conversion For A Smaller Furnace Yeilds Big Results

Applications of oxy-fuel to glass melting furnaces had until recently only been the domain of very large tanks. But oxy-fuel is proving to be ideal for just about everyone, including smaller furnaces and day tanks.