Origin Of Colour In Iron And Manganese Containing Glasses Investigated By Synchrotron Radiation

The origin of colour in medieval glasses from Northern Europe has been shown to be an artifact of the oxidation states of small concentrations of Fe and Mn added as impurities in the alkali source.