Optimizing Glaze Transparency By Design

Mixture design methodology was used to optimize a ceramic frit composition, commonly used in fabricating transparent glazes for single-fired tile, by minimizing immiscible liquid-phase separation in the resulting glaze.

Author
R Gimeno Et Al
Origin
Fritta Sl, Spain
Journal Title
Am Ceram Soc Bull 75 10 1996 71-75
Sector
Enamels
Class
E 25