Optimization Of Glass Batch Preparation

An optimum cyclogram for dosing small additives in glass batch preparation is considered, taking into account indirect control of mixing quality based on the mixer motor power. A scheme of preparation and introduction of a premix of selenium and cobalt oxide with a filler is described.

Author
V V Efremenkov & V P Chalov
Origin
Bspkto Stekoavtomatika Jsc, Russia
Journal Title
Glass And Ceramics 57 1-2 2000 37 - 39