Optimising Float Glass Processing Procedures

The Grezebach float optimisation system, developed over many years, is more than merely a cutting optimisation system. Line capacity optimisation helps to use the equipment to best advantage, order pool optimisation helps to find the most economic production mix and diagnostic routines monitor and log failures "in the bud."

Author
Un-named
Origin
Grenzebach Maschinenbau Gmbh
Journal Title
Glass 72 1 1995 17