Optimising Batch Formulation And Furnace Operation

This article addresses the need to establish and maintain good control over the batch and glass redox chemistry, as part of the overall production process to increase product quality and reduce bottom-line unit costs.

Author
D Myers And R Hulme
Origin
Calumite Int Ind, Uk
Journal Title
Glass Prod Tech Int 1995 31-34