Optimised Glass Cutting

The Perfect Cut software developed the Italian company R.O., has proven effective in reducing waste. Cutting solutions are created or modified according to requirements, while a CAD system allows management of cutting shaped glass. The system is simple to use and has all the functions specific to the glassworking industry.

Author
D Aimonetto
Origin
R.O. Italy
Journal Title
Glass-Tech Int 6/97 111-114
Sector
Flat glass
Class
F 799