Optical Flint Glass With Enhanced Transmission In The Ultraviolet Region

The possibility of preparing lead phosphate flint glasses with high transmission (up to 95% for a 10-mm layer at the wavelength of 350-360nm) and a high refractive index is shown. The developed glasses are recommended for optical systems.

Author
O E Yabluchanskii Et Al
Origin
Di Mendeleev Russian Chem Eng University, Moscow
Journal Title
Glass & Ceramics 53 5-6 1996 204-206
Sector
Special Glass
Class
S 1582b