Operation Of A Glass- Melting Furnace With A Heat-Insulating Melting Tank

The operating advantages of a glass melting furnace with a thermally insulated melting tank are considered. A scheme of thermal insulation is presented. The efficiency of the heat insulation of the melting tank in the production of glass with decreased light transmission is noted.