Opacification Of Glass By Fluorides

Practical melting tests carried out by the author and published in Sprechaal and GEKT showed that besides CaF2 and NaF2 other fluorides (BaF2, MgF2 and KF) also contribute in rendering a glass opalscent.

Author
F. Jochmann.
Origin
Unknown
Journal Title
Glas-Email-Keramo-Technik 1960 11 (5) 152-158