The Kunzmann Group, from Dasing in Upper Bavaria produces mineral water, soft drinks, fruit juices, wine and mulled wine - achieving steady growth rates. According to Jurgen Kunzmann, the company's MD, one thing is set in stone at the company: no beverages are ever going to be bottled in PET. Its success has been its own vindication. So as to match the production capacity to current growth, the company has recently installed a new Krones line for returnable glass bottles. The project is described in this article.
Origin
Unknown
Journal Title
Krones Magazine 1/2017 74-81
Sector
Packaging Abstracts
Class
PA 1363