Online Sampling And Analysis Of Glass Cullet

This paper looks at quality requirements for glass cullet and the technology behind cullet processing. The article also looks at the limits set out in most European countries.

Author
F Moberg
Origin
Mobergs Processkontroll Ab, Sweden
Journal Title
Glasteknisk Tidskrift 50 1 1995 22-26
Sector
General
Class
G 1336