Online Measurements Of Redox Properties In Glass Forming Melts

This article looks at measurements of redox properties in glass forming melts. Thermodynamic data for various polyvalent ions is tabled.

Author
C Russel
Origin
Universitat Erlangen-Nurnberg, Germany
Journal Title
The Glass Researcher 10Th Anniversary Collection 1986/96 24-25
Sector
General
Class
G 2689