Numerical Modeling Of Reacting Liquid Glass Layer In An Advanced Glass Melter

A numerical model has been developed to describe the behaviour of the liquid layer formed by the dissolution of solid particles in the liquid flow and diffusion to form glass that occurs in an Advanced Glass Melter.