Nonlinear Viscous Flow In Glass Forming

The role of viscosity in glass forming is discussed with particular reference to high rates of shear. The effect of phase separation is also considered.

Author
J H Simmons, Cj Simmons
Origin
University Of Florida
Journal Title
Ceramic Bulletin 1989 68 11 1949-1955