Nonlinear Optical Properties Of B203 Based Glasses: Binary Ag20-B203 And Ternary Agx-Ag20-B203 (X=Cl, Br And I) Glasses

The third order nonlinear optical susceptibilities X(3) of AgX-Ag20-B203 (X=Cl, Br and I) glasses have been measured by the third harmonic generation (THG) method with special attention to highly polarisable cations and halide anions contained in these glasses.

Author
K Terashima Et Al
Origin
Kyoto University, Japan
Journal Title
Phys Chem Glasses 37 4 1996 129-133
Sector
Special Glass
Class
S 1040