Nondestructve Analysis By Neutron Activation Of Refractory Materials And Of A Glass (In French)

Neutron activation analysis has been carried out on six refractory samples containing alumina or zirconia and also on a sample of float glass. After thermal neutron irradiation the radioactivity of the samples was measured by gamma ray spectrometry. It was possible to determine 22 elements without chemical separation.