Non-Contact Thickness Measurement

The non-contact measurement of wall thickness becomes more and more important due to the process control of glass manufacturing. VMA has designed a series of opto-electronic thickness gauges for tubes, flat glass, thin-walled blown hollow glass as well as for container glass. The results of long-term tests are available.

Author
Dr B Kiessling
Origin
Vma-Gesellschaft Fur Visuelle Messtechnik Und Automatisierung Gmbh
Journal Title
International Glass Review Spring/Summer 1996 133, 135-137
Sector
Container glass
Class
C 948