Non-Contact Level Measurement In The Glass Making Industry

This article describes two examples from the glass making industry - the monitoring of the raw material level in silos and on conveyors, as well as the maintenance of a constant level in a glass furnace.

Author
Dr P Berrie
Origin
Endress & Hauer, Germany
Journal Title
International Glass Review Spring/Summer 1996 75, 77-79