Non-Contact Ir Line-Scanners For Accurate Control

In order to achieve product uniformity, non-contact temperature measuring methods are increasingly being used and are an accepted and important technique for process control and quality. This article looks at some of the benefits and existing applications.

Author
P Ott
Origin
Raytek Gmbh, Germany
Journal Title
Glass-Tech Int 3/99 105-107
Sector
Flat glass
Class
F 964