Nickel Sulphide Inclusions - Important Issues For The Designer

This paper focuses on the current position and the issues available to designers. As well as discussing the key issues, methods of predicting further breakage are presented so that, based on the known success rates of heat soaking, confidence can be gained in using the product when the risks are taken into account.