Nickel Sulphide Inclusions In Glass: An Example Of Microcracking Induced By A Volumetric Expanding Phase Change

Microcracking about inclusions of nickel sulphide in soda-lime glass has been studied.

Author
M V Swain
Origin
St Gobain Recherche, France
Journal Title
J Mat Sci 16 1981 151-158
Sector
Flat glass
Class
F 506

Request article (free for British Glass members)

Nickel Sulphide Inclusions In Glass: An Example Of Microcracking Induced By A Volumetric Expanding Phase Change
J Mat Sci 16 1981 151-158
F 506