New York State: Birthplace And Cradle Of High-Technology Ceramics And Glasses

Since the turn of the century, New York State has been the home of countless ceramic and glass companies. These companies and other NYS industries have given rise to many of the greatest accomplishments in high-technology ceramic and glass materials in the 20th century. Examples of these are cited.