New, Modular Laminating Plants

Elettromeccanica Bovone has decades of experience in machinery and equipment for flat glass processing. The company has launched a new production line for laminated glass to suit modern world markets. The modular design of the line opens up a wide range of alternatives regarding the dimensions, thickness and layering of the glass. Another advantages is that both the ovens and the autoclave can be fed by gas, which results in low overall plant installation and maintenance costs.