Signo Glassguard brings the power of nanotechnology to preserving glass quality. The product develops strong but inert chemical bonds with the underlying glass substrate - effectively becoming an integral part of the surface, says Signo. The smooth, anti-stain, non-discolouring layer formed is crystal clear, UV stable, chemically inert and extremely durable, having both hydrophobic and oleophobic capabilities. It will not discolour, peel or flake and is unaffected by extremes of temperatures from -20C to +350 deg C, says the company.