New Generation Refractories For Regenerators

The life-span of high-performance glass tanks depends upon the efficiency of regenerators. New design checker bricks increase tank life and generate higher temperature clean preheated air for firing. Energy can be saved in glass units by correction seletion and design of refractories, and insulationof furnaces and regenerators. In this paper experts from Tata Refractories (India) Ltd give guidelines for selection and design.