New Fact Sheet From Cetie

The European bottling association CeTIE has produced a new document: "Recommendation Datasheet FS 16 - July 2020 - Pressure resistance test procedures for products bottled with aluminium screw caps." the fact sheet provides test methods which enable evaluating of the level of sealing obtained with an aluminium screw cap applied on a filled glass bottle. Different tests are proposed covering the various objectives for such a test, either for product development, for routine checks during filling operations or for troubleshooting.