New Developments In Nox Control - The Pilkington 3R Process

An outline of Pilkington's response to increasing environmental pressures from NOx emissions. Although the glass industry is only a minor contributor to total mass emissions, its furnaces often emit NOx at high concentrations. This paper outlines the 3R process for NOx reduction.

Author
G Evans And I W N Shulver
Origin
Pilkington Glass Products
Journal Title
Glass Prod Tech Int 1995 74-76
Sector
Flat glass
Class
F 470