New Channels To Be Added To The Online Standard Float Inspection System: Reflected Distortion, Tin Detection And Coating Inspection

This article looks at the development of new channels, especially for measuring reflected distortion, detection of tin or coating defects is the solution to meet increased quality requirements for float glass manufacturers.